OK Tigrod 13.09

A copper coated, low alloyed, molybdenum (0,5% Mo) rod for GTAW of creep resistant steels of the same type, such as pipes in pressure vessels and boilers with a working temperature of up to about 500 ᄚC.

Request A Quote

Highlights

Process

Specifications
Classifications EN ISO 636-A : W 46 2 2Mo
EN ISO 636-A : W 2Mo
EN ISO 21952-A : W MoSi
EN ISO 21952-B : W 52 1M3
SFA/AWS A5.28 : ER70S-A1 (ER80S-G)
Approvals CE : EN 13479
DB : 42.039.08
DNV-GL : III YMS (I1)
UKCA : EN 13479
VdTÜV : 04950
Alloy Type Low alloyed steel (0.5 % Mo)
Shielding Gas I1 (EN ISO 14175)
Tensile_Properties
Testing Condition Yield Strength Tensile Strength Elongation
EN Ar (I1)
As Welded 490 MPa 600 MPa 30 %
PWHT
1 hour(s) 620 °C
450 MPa 550 MPa 31 %
AWS Ar (I1)
As Welded 520 MPa 620 MPa 27 %
PWHT
1 hour(s) 620 °C
510 MPa 610 MPa 28 %
Charpy Testing
Testing Condition Testing Temp Impact Value
EN Ar (I1)
As Welded 20 °C 180 J
PWHT
1 hour(s) 620 °C
20 °C 190 J
As Welded -20 °C 160 J
PWHT
1 hour(s) 620 °C
-20 °C 170 J
As Welded -40 °C 90 J
As Welded -60 °C 25 J
AWS Ar (I1)
PWHT
1 hour(s) 620 °C
-20 °C 220 J
As Welded -29 °C 150 J
As Welded -46 °C 130 J
Typical Weld Metal Analysis %
C Mn Si S P Mo Cu
0.1 1.1 0.7 0.015 0.015 0.5 0.2
Typical Wire Composition %
C Mn Si Ni Cr Mo
0.094 1.09 0.61 0.05 0.05 0.45
Description Product Number
OK Tigrod 13.09 1.6 × 1000 mm 5 kg 130916R150
OK Tigrod 13.09 2.0 × 1000 mm 5 kg 130920R150
OK Tigrod 13.09 2.4 × 1000 mm 5 kg 130924R150
OK Tigrod 13.09 3.2 × 1000 mm 5 kg 130932R150